Your Whitening Toothpaste Says RDA 117. What Does That Number Actually Cost You?

Created on 11.25
A formulator in Guangzhou sent me two whitening pastes in June. Same base, same fluoride, same flavour. One used our T101 abrasive at 18 percent. The other used a coarser grade at the same loading. The first read RDA 117 on the dentin method. The second read 168. Both were labelled "whitening" and both were selling.
He asked which one was better. That is the wrong question, and it is the question almost everyone asks. The right one is what the number costs you in enamel, in claims, and in the tube you actually fill.

What RDA is measuring, and what it is not

RDA is radioactively labelled dentin abrasion. A treated dentin slab is brushed in a machine under a fixed load and stroke count, and the amount of dentin worn away is compared with a reference slurry. The result is a number, not a verdict.
Most mainstream pastes sit between 70 and 150. Below 70 you are in the "low abrasion" zone, which sounds safe until you look at cleaning. Above 150 you start to see dentin loss in patients who brush hard or often, and in people with exposed roots after gum recession.
RDA does not tell you how well the paste removes stain. That is PCR, the pellicle cleaning ratio, measured on stained pellicle in vitro. A paste can have RDA 90 and PCR 110, or RDA 130 and PCR 95. The two numbers move in the same direction only if the particle shape and hardness are the same.

Where our T101 sits

ZLDIO T101 is a precipitated abrasive with D50 around 10 to 14 microns, oil absorption up to 125 g per 100 g, whiteness above 93, and transmittance above 90 percent. On the standard dentin method it reads RDA 117, PCR 80. Surface roughness on a brushed acrylic block comes out at Ra 0.336 micron.
That profile is a middle-of-the-road whitening abrasive. It cleans stains without going into the aggressive range, and it stays translucent enough for a gel base if the rest of the formula cooperates.
T113 is the same platform with oil absorption of 80 to 100. It cleans a little less and sits better in a transparent gel. If you are building a clear whitening gel, T113 is usually the easier starting point, and you make up the cleaning with the surfactant system rather than with more abrasive.

Particle size is only half the story

Two silicas with the same D50 can read 20 points apart on RDA if the particle shape differs. Angular, hard particles cut. Rounded, porous particles polish. Our process gives a fairly rounded precipitated particle, which is why a 12 micron D50 lands at 117 instead of 150.
The size distribution matters too. A narrow distribution gives predictable abrasion. A wide one puts a few large particles in every gram, and those large particles do most of the scratching while contributing little to cleaning.
Ask for D10, D50 and D90, not just the average. And ask whether the D90 is a laser number or a sieve residue. A 325 mesh pass of 98 percent tells you very little about the top end of a 12 micron powder.

What the base does to the number

RDA is measured on the finished paste, not on the powder. The same silica can read 117 in one formula and 135 in another. Three things move it.
Humectant level is the first. A high glycerin paste is more viscous and holds the particles against the dentin longer per stroke. Water-heavy gels release them faster.
Thickener is the second. A silica thickener like TY2 or TC15 adds its own fine particles, and those fine particles contribute to cleaning without adding much abrasion. That is usually a good trade.
The third is pH and fluoride system. Sodium fluoride at pH 7 is gentle on silica. Stannous fluoride is a different animal, and I will come back to it.

The stannous problem

Stannous fluoride is popular again because of gingivitis claims. It also hydrolyses in water and can adsorb onto silica surfaces, which drops the free fluoride number and can discolour the paste over time.
If you are formulating with stannous, ask for a fluoride compatibility figure. Our T101 holds above 90 percent free fluoride in a standard NaF system after four weeks at 40 degrees. Stannous is harder. Run your own stability at 40 degrees for eight weeks and measure free fluoride at week zero, four and eight before you commit to a launch date.
Do not assume that a silica that works with NaF will work with stannous. The surface chemistry is different and the failure mode is silent. The paste looks fine and the fluoride number quietly drops.

What "whitening" can mean on a label

Most whitening toothpaste does not bleach. It removes extrinsic stain with abrasive and surfactant, and it prevents new stain with pyrophosphate or similar. That is a legitimate claim in most markets if you can support it with an in vitro stain removal test.
Peroxide pastes are a different regulatory category in many countries. If you are exporting, check the destination rules before you put the word whitening on the carton. A paste that is fine in one market can need a different notification in another.
What you should not do is print an RDA number on the pack unless you have measured it on the finished product, in a qualified lab, on the batch you are selling. RDA on the powder datasheet is a starting point, not a label claim.

Scale-up problems that show up late

Powder feeding is where most plants lose the formula. Silica at 0.3 g/ml bulk density does not flow like chalk. A volumetric feeder will run 5 to 8 percent rich at the start of a batch and lean at the end as the hopper empties.
Use a gravimetric feeder with a flexible hopper wall, or a vacuum loader with a loss-in-weight cycle. And check the paste density after vacuum, not before. Entrained air can make a 1.45 g/ml paste read 1.38, and the tube fill weight will be wrong even though the formula is right.
Mixing order matters as well. Disperse the silica into the humectant before you add water. If you add water first, the silica hydrates on the outside of the lump and you get fish eyes that survive the rest of the batch.

A test plan that fits a launch schedule

Week one: RDA and PCR on the finished paste, plus pH and viscosity at three temperatures. Week two: fluoride availability and a 40 degree stability pull. Week three: a brushing test on acrylic blocks for Ra, and a stain removal comparison against your current SKU.
If you change the abrasive grade after week two, start again. Abrasive changes move RDA, PCR, viscosity and fluoride availability at the same time, and a partial retest will not catch the interaction.

Frequently asked questions

Q1. What RDA should a whitening toothpaste target? 100 to 130 is a workable band for a mainstream whitening paste. Below 90 the cleaning claim gets hard to support, above 150 the enamel story gets hard to defend.
Q2. Is RDA measured on the powder or the paste? The paste. The powder datasheet number is a guide for formulation, not a claim you can print.
Q3. Can I lower RDA by reducing the silica loading? Yes, but you also lower PCR. If you need the cleaning, change to a softer or more porous grade instead of cutting the dose.
Q4. Does particle size determine RDA? It is the biggest lever, but shape and distribution matter as much. A narrow, rounded 12 micron particle can read lower than an angular 10 micron one.
Q5. What is a good PCR number? 80 to 100 covers most whitening claims. Above 110 you are in strong stain removal territory and should check the abrasion side carefully.
Q6. Why does my paste darken with stannous fluoride? Stannous ions adsorb on silica and oxidise. Check the silica surface treatment and the paste pH, and run an eight-week 40 degree test before launch.
Q7. Can silica replace calcium carbonate one for one? Not by weight. Silica is lighter and more porous, so you need less, and the rheology changes. Reformulate the humectant and thickener together.
Q8. How do I check dispersion in the finished paste? Spread a thin film on a glass slide and look for specks under a light box. More than two specks per square centimetre means the dispersion step needs work.
Q9. Does the thickener silica add abrasion? Mildly. Fine thickener particles contribute to cleaning and to RDA, but far less than the abrasive fraction.
Q10. What sieve residue should I ask for? 325 mesh pass of 98 percent minimum for an abrasive grade. Anything lower means coarse particles that will show up as scratches.
Q11. Is there a silica grade for sensitivity toothpaste? Yes, use a lower loading of a fine abrasive and lean on the desensitising agent. RDA under 70 is achievable without losing all cleaning if the particle is porous.